                            induction rod forging 12cm (steel rods) steel bars by um-120ab-mf
                            
                              induction rod forging 12cm steel bars by 120KW machineinduction forging 12cm (steel rod) steel bars by 120KW machine-1induction forging 12cm steel bars by 120KW machine-2induction forging 12cm steel rod (steel bars) by 120KW machine-3induction rod forging … 
- 
                            medium frequency for induction heating rods
                            
                              Machine: UM-120AB-MFmedium frequency for induction heating rods 
- 
                            induction heating eight steel rods
                            
                              Heating Eight Steel Rods Objective Heat eight steel rods simultaneously to 212F (100C) for a molding operation.Material 8 Steel Rods measuring 1/2 (12.7mm) in diameter and 14 (355.6mm) long held in place by 2.5” (63.5mm) diameter Teflon end plates.Tempera… 
- 
                            induction forge steel rods
                            
                              Objective To heat the ends of steel rods to 1800F prior to a forging operation. Processing of the rods includes heating, pressing in a two part die to forge the push rod end, and a final heating in a channel coil to temper the rods and relieve the forging … 
- 
                            induction preheating titanium rods
                            
                              Objective To heat titanium rod blanks prior to forging into a turbine blade. Material Titanium rod blanks 0.591″(15.01mm) OD by 11.8″(299.7mm) long Temperature 2030F(1110C) Frequency 64 kHz Equipment • Power of 45kW induction heating system equipped… 
- 
                            induction annealing tungsten rods
                            
                              Objective To heat customer-supplied rods of various diameters (0.14 inch to 0.49 inch) to 4170F (2300C) at 2-4 feet per minute Material Tungsten and Molybdenum; Tests are run in an atmosphere of Nitrogen or Hydrogen avoid oxidation of the materials. Temp… 